Property |
Test method |
Unit |
HBHZD150 | HBHZD200 |
Mass per unit area |
ISO9073-1 |
g/㎡ |
260±40 |
280±40 |
Thickness |
ISO9073-2 |
mm |
1.5±0.6 |
2.0±0.6 |
Tensile strength |
ISO9073-3 |
N/cm |
≥40 |
≥40 |
Elongation |
ISO9073-3 |
﹪ |
≥12 |
≥12 |
Swelling speed |
Q/1002WHS001-2012 |
mm/min |
≥8 |
≥8 |
Swelling height |
Q/1002WHS001-2012 |
mm/3min |
≥12 |
≥12 |
Surface resistivity |
DINIEC167 |
Ω |
﹤1500 |
﹤1500 |
volume resistivity |
DIN54345 |
Ω.cm |
﹤1×106 |
﹤1×106 |
Short term stability |
Q/1002WHS001-2012 |
℃ |
230 |
230 |
Long term stability |
Q/1002WHS001-2012 |
℃ |
90 |
90 |
Moisture content |
Q/1002WHS001-2012 |
﹪ |
≤9 |
≤9 |